MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Rogers Arlon 22122R079 0.079" Cured Silicone Rubber and FEP Film Laminate
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP); Thermoset; Silicone; Silicone Rubber

Material Notes: Design/Construction:
  • Interleave: 3 mil Polyethylene
  • Side 1: Cured Silicone Rubber
  • Substrate: 0.005" FEP Film

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 127 microns5.00 milSubstrate; Arlon SQA-TMS-003
 1880 microns74.0 milSide 1; Arlon SQA-TMS-003
 2010 microns79.0 milOverall Thickness; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565Silicone Property; ASTM D2240
Tensile Strength 7.433 MPa1078 psiSilicone Property; ASTM D412
Elongation at Break 341 %341 %Silicone Property; ASTM D412
Tear Strength 16.0 kN/m91.0 pliDie B, Silicone Property; ASTM D624
Peel Strength 2.07 kN/m11.8 pliSilicone to FEP Bond Strength
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 19.1 kV/mm>= 486 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 60.0 Month
@Temperature 21.1 °C
60.0 Month
@Temperature 70.0 °F
 
Descriptive Properties
ColorRed
 TransparentSubstrate
Total Product Weight (oz/yd2)77Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 26122P020 0.020" Cured Silicone Rubber/Laminated PTFE Film

PARL9710 / 148863

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.