MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Mobility and Materials Zytel® HTNFR42G30NH NC010 PA-GF30FR(40)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes:

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³DAM; ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 138 MPa20000 psiDAM; ISO 527-1/-2
Elongation at Break 1.8 %1.8 %DAM; ISO 527-1/-2
Tensile Modulus 10.6 GPa1540 ksiDAM; ISO 527-1/-2
Flexural Strength 216 MPa31300 psiDAM; ISO 178
Flexural Modulus 11.2 GPa1620 ksiDAM; ISO 178
Charpy Impact Unnotched 4.60 J/cm²
@Temperature 23.0 °C
21.9 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VDAM; IEC 60112
 >= 600 V
@Thickness 3.00 mm
>= 600 V
@Thickness 0.118 in
DAM; UL 746A
 
Thermal PropertiesMetricEnglishComments
Melting Point 315 °C599 °Ffirst heat; ISO 11357-1/-3
UL RTI, Electrical  130 °C
@Thickness 0.400 mm
266 °F
@Thickness 0.0157 in
UL 746B
 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL 746B
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746B
UL RTI, Mechanical with Impact  115 °C
@Thickness 0.400 mm
239 °F
@Thickness 0.0157 in
UL 746B
 115 °C
@Thickness 1.50 mm
239 °F
@Thickness 0.0591 in
UL 746B
 120 °C
@Thickness 3.00 mm
248 °F
@Thickness 0.118 in
UL 746B
UL RTI, Mechanical without Impact  125 °C
@Thickness 0.400 mm
257 °F
@Thickness 0.0157 in
UL 746B
 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
DAM; UL 746B
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746B
Flammability, UL94 V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
DAM; IEC 60695-11-10
Glow Wire Ignition Temperature  750 °C
@Thickness 0.400 mm
1380 °F
@Thickness 0.0157 in
DAM; IEC 60695-2-12
 800 °C
@Thickness 1.50 mm
1470 °F
@Thickness 0.0591 in
DAM; IEC 60695-2-13
 825 °C
@Thickness 3.00 mm
1520 °F
@Thickness 0.118 in
DAM; IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
DAM; IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
DAM; IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
DAM; IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature >= 325 °C>= 617 °FInjection; -
 <= 335 °C<= 635 °FInjection; -
Mold Temperature >= 110 °C>= 230 °FInjection; -
 <= 130 °C<= 266 °FInjection; -
Drying Temperature 100 °C
@Time 21600 - 28800 sec
212 °F
@Time 6.00 - 8.00 hour
Dehumidified Dryer; Injection Molding; Injection
Moisture Content 0.10 %0.10 %Injection
 
Descriptive Properties
AdditiveRelease agent
Delivery formPellets
Part Marking Code>PPA-GF30FR<SAE J1344
 PA-GF30FR(40)ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA-GF30FR(40)ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant
RTP Company RTP 4005 FR  Polyphthalamide (PPA) Glass Fiber 30% - Flame Retardant
LNP Thermocomp® UF-1006 FR HS LEX BK8-115 Polyphthalamide, Glass Fiber Reinforcement

PDSY5448s / 239851

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.