MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Extruded

Material Notes: ENSILON materials have high mechanical strength and superior resistance to wear and organic chemicals.

Ensilon grades have been replaced by Tecamid.

Information supplied by Ensinger, Inc.

Key Words: PA6/6; Polyamide 6/6
Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Water Absorption 1.2 %1.2 %24 hrs.; ASTM D570
Water Absorption at Saturation 8.5 %
@Temperature 23.0 °C
8.5 %
@Temperature 73.4 °F
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7979ASTM D785
Hardness, Rockwell R 120120ASTM D785
Tensile Strength at Break 85.5 MPa12400 psiASTM D638
Elongation at Break 90 %90 %ASTM D638
Flexural Yield Strength 117.2 MPa17000 psiASTM D790
Flexural Modulus 2.80 GPa406 ksiASTM D790
Izod Impact, Notched 0.640 J/cm1.20 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 4.0
@Frequency 60 Hz
4.0
@Frequency 60 Hz
50% RH; ASTM D150
Dielectric Strength 11.8 - 15.7 kV/mm300 - 399 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear  81.0 µm/m-°C
@Temperature -20.0 - 200 °C
45.0 µin/in-°F
@Temperature -4.00 - 392 °F
ASTM D696
 90.0 µm/m-°C
@Temperature 93.3 - 238 °C
50.0 µin/in-°F
@Temperature 200 - 460 °F
ASTM D696
Maximum Service Temperature, Air 99.0 °C210 °FLong Term
 179 °C354 °FShort Term
Deflection Temperature at 0.46 MPa (66 psi) 235 °C455 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet)
Asahi Kasei Thermylon® N3-25FG-2726 PA66-GF25
BASF Ultramid® 1000-11 NF2001 PA66 (Dry)
Celanese CoolPoly® D3612 Thermally Conductive Polyamide (PA66/6)
Envalior Akulon® S223-D PA66, Dry

PENS39 / 35985

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.