MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company EMI 161 Polypropylene (PP), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Stainless Fiber, EMI

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccASTM D 792
Water Absorption 0.010 %
@Time 86400 sec
0.010 %
@Time 24.0 hour
ASTM D 570
Additive Loading 10 %10 %Primary Additive
Linear Mold Shrinkage 0.0090 - 0.014 cm/cm
@Thickness 3.20 mm
0.0090 - 0.014 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 20.7 MPa3000 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 1.45 GPa210 ksiASTM D 638
Flexural Strength 27.6 MPa4000 psiASTM D 790
Flexural Modulus 1.24 GPa180 ksiASTM D 790
Izod Impact, Notched 2.67 J/cm
@Thickness 3.20 mm
5.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 10.7 J/cm
@Thickness 3.20 mm
20.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.10 - 10 ohm-cm0.10 - 10 ohm-cmASTM D 257
Surface Resistance 10 - 1000 ohm10 - 1000 ohmESD STM11.11
Surface Resistivity per Square 100 - 10000 ohm100 - 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 2.0 sec<= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Shielding Effectiveness  46 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
46 dB
@Thickness 0.0787 in,
Frequency 1e+9 Hz
ASTM D 4935
 46 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
46 dB
@Thickness 0.0787 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 46 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
46 dB
@Thickness 0.0787 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 47 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
47 dB
@Thickness 0.0787 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 48 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
48 dB
@Thickness 0.0787 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 53 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
53 dB
@Thickness 0.0787 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 58 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
58 dB
@Thickness 0.118 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 61 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
61 dB
@Thickness 0.118 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 63 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
63 dB
@Thickness 0.118 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 64 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
64 dB
@Thickness 0.118 in,
Frequency 1e+9 Hz
ASTM D 4935
 68 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
68 dB
@Thickness 0.118 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 70 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
70 dB
@Thickness 0.118 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 221 °C380 - 430 °F
Mold Temperature 37.8 - 51.7 °C100 - 125 °F
Drying Temperature 79.4 °C
@Time 7200 sec
175 °F
@Time 2.00 hour
Moisture Content 0.10 %0.10 %
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company EMI 162 Polypropylene (PP) Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1060.7 FR Polybutylene Terephthalate (PBT), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
RTP Company EMI 2561 FR Polycarbonate/ABS Alloy (PC/ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
RTP Company ESD C 780 High Density Polyethylene (HDPE), Carbon Fiber - ESD Protection - Electrically Conductive
RTP Company RTP 799 X 112538 High Density Polyethylene (HDPE), Permanently Anti-static - Masterbatch

PQZWA1354 / 90774

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.