MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

INEOS Styrolution Terblend® N NG-02 UV ABS / PA, 8% Glass filled
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced

Material Notes: Terblend N NG-02 UV is an 8% glass fiber reinforced (UV stabilized) ABS/PA blend with enhanced dimensional stability and rigidity.
  • High dimensional stability
  • Enhanced rigidity
  • Enhanced softening temperature
  • Glass fiber reinforced (8%)

Information provided by Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.1 %
@Temperature 23.0 °C
1.1 %
@Temperature 73.4 °F
50% RH; ISO 62
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inISO 294-4
Melt Flow 30 g/10 min
@Load 10.0 kg,
Temperature 240 °C
30 g/10 min
@Load 22.0 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 95.0 MPa13800 psiISO 2039-1
Tensile Strength, Yield 55.0 MPa7980 psiISO 527
Elongation at Break 4.0 %4.0 %ISO 527
Elongation at Yield 3.0 %3.0 %ISO 527
Tensile Modulus 3.30 GPa479 ksiISO 527
Flexural Strength 80.0 MPa11600 psiISO 178
Flexural Modulus 2.85 GPa413 ksiISO 178
Izod Impact, Notched (ISO)  3.00 kJ/m²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 6.00 kJ/m²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched  2.50 J/cm²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 3.50 J/cm²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.013
@Frequency 1e+6 Hz
0.013
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C33.3 µin/in-°FISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FISO 75
Vicat Softening Point  108 °C
@Load 5.10 kg
226 °F
@Load 11.2 lb
50°C/h; ISO 306
 170 °C
@Load 1.02 kg
338 °F
@Load 2.25 lb
50°C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 270 °C464 - 518 °FISO 294
Mold Temperature 40.0 - 80.0 °C104 - 176 °FISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® T85 XF Polycarbonate + ABS
INEOS Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Dry)
Trinseo MAGNUM™ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
BASF Ultraform® H 4320 Q600 POM
ExxonMobil PP7855E1 Polypropylene Homopolymer

PBASF9034A / 159696

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.