Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Excellent resistance to creep under load, and maintains the inherent chemical and electrical properties associated with polyesters. |