MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

A. Schulman BMC 1902 Mineral Filled Alkyd
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Alkyd (Polyester), Molded, Mineral Filler

Material Notes: BMC 1902 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression molding. It was developed primarily for applications requiring very good impact and flexural strengths.

Typical applications include phase barriers, connector bases, switch cases and circuit breaker handles

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.08 g/cc2.08 g/cc
Water Absorption 0.23 %0.23 %24 hours, 23°C
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 60 - 8060 - 80
Flexural Strength 145 - 179 MPa21000 - 26000 psi
Compressive Strength 152 - 179 MPa22000 - 26000 psi
Izod Impact, Notched 2.14 - 3.20 J/cm4.00 - 6.00 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 7.1
@Frequency 60 Hz
7.1
@Frequency 60 Hz
Dielectric Strength 11.8 kV/mm300 kV/inShort Time
Dissipation Factor 0.030
@Frequency 60 Hz
0.030
@Frequency 60 Hz
Arc Resistance 180 sec180 sec
Comparative Tracking Index >= 500 V>= 500 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °F
Flammability, UL94  HB
@Thickness 6.35 mm
HB
@Thickness 0.250 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Mold Temperature 138 - 166 °C280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Crastin® LW9320 BK851 PBT+SAN-GF20
Celanese Crastin® CE15330 BK010 PBT-GF30FR(17)

PBMC057 / 27240

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.