MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil HDP 8660.29 High Density Polyethylene (HDPE), Copolymer Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Copolymer Film Grade

Material Notes: HD 8660 series are high density hexene copolymers designed to offer superior toughness and stiffness.  They are ideally suited for applications that require the optimum balance of low temperature toughness, creep resistance, stiffness, ESCR, and tear properties. 

Availability: Latin America, North America. 

Additive:  long term UV-15 stabilizer: yes. 

Applications:  industrial products, intermediate bulk containers, large agricultural tanks.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.941 g/cc0.0340 lb/in³ASTM D1505
ESCR 100% Igepal® 560 hour560 hourF50; ASTM D1693A
ESCR 10% Igepal® 40 hour40 hourF50; ASTM D1693A
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
mod; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 19.3 MPa2800 psi2.0 in/min; ASTM D638
Elongation at Yield 10 %10 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 896 MPa130000 psiASTM D790B
Impact Test  92.2 J
@Thickness 3.17 mm,
Temperature -40.0 °C
68.0 ft-lb
@Thickness 0.125 in,
Temperature -40.0 °F
ARM
 258 J
@Thickness 6.35 mm,
Temperature -40.0 °C
190 ft-lb
@Thickness 0.250 in,
Temperature -40.0 °F
ARM
 
Thermal PropertiesMetricEnglishComments
Melting Point 129 °C264 °FPeak; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 57.2 °C135 °Funannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C100 °Funannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Paxon™ HYA021L High Density Polyethylene (HDPE), Copolymer Film Grade
ExxonMobil Paxon™ BA54-030 High Density Polyethylene (HDPE), Copolymer Film Grade
ExxonMobil HDP 8760.29 High Density Polyethylene (HDPE), Copolymer Film Grade
ExxonMobil HD 7957.04 High Density Polyethylene (HDPE), Film Grade
Dow HDPE 65053N High Density Polyethylene

PEX98884 / 238266

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.