System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Mocom (ALBIS) ALTECH® PP-B A 3030/500 GB30 Polypropylene Heterophasic Copolymer, 30% Glass Bead Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene Glass Bead Filled
Material Notes:
Base Polymer: Polypropylene Heterophasic Copolymer
Filler/Additive System: 30% glass beads
Market Segment: Various
Typical Applications: Various
Information provided by Albis Plastics
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.10
g/cc
0.0397
lb/in³
ISO 1183
Linear Mold Shrinkage, Flow
0.0080
-
0.010
cm/cm
@Time 86400 sec
0.0080
-
0.010
in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse
0.010
-
0.012
cm/cm
@Time 86400 sec
0.010
-
0.012
in/in
@Time 24.0 hour
ISO 294-4
Melt Flow
8.0
g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature
<=
30.0
°C
<=
86.0
°F
dry, protected from light
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
12.0
MPa
1740
psi
ISO 527
Tensile Strength, Yield
16.0
MPa
2320
psi
ISO 527
Elongation at Break
70 %
70 %
ISO 527
Elongation at Yield
5.3 %
5.3 %
ISO 527
Tensile Modulus
1.40
GPa
203
ksi
ISO 527
Flexural Strength
24.0
MPa
3480
psi
ISO 178
Flexural Modulus
1.35
GPa
196
ksi
ISO 178
Charpy Impact Unnotched
6.00
J/cm²
28.6
ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched
0.600
J/cm²
2.86
ft-lb/in²
ISO 179/1eA
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
67.0
°C
153
°F
ISO 75-1/-2
Vicat Softening Point
64.0
°C
147
°F
B50; ISO 306
Processing Properties
Metric
English
Comments
Melt Temperature
200
-
270
°C
392
-
518
°F
Injection molding
Mold Temperature
20.0
-
90.0
°C
68.0
-
194
°F
Injection molding
Drying Temperature
80.0
-
120
°C
@Time 7200 - 10800 sec
176
-
248
°F
@Time 2.00 - 3.00 hour
in a dry air (desiccant) dryer
80.0
-
120
°C
@Time 7200 - 14400 sec
176
-
248
°F
@Time 2.00 - 4.00 hour
air circulating dryer
Descriptive Properties
Base Polymer
Polypropylene Heterophasic Copolymer
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PALBIS8838 / 242897
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.