MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eurotec® Tecodur® PB70 GR30 NL100 IL PBT, 30% glass fiber reinforced, impact modified, natural
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled; Polybutylene Terephthalate (PBT), Impact Grade

Material Notes:

Information provided by Eurotec®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³ISO 1183
Moisture Absorption 0.100 %
@Temperature 23.0 °C
0.100 %
@Temperature 73.4 °F
50% RH; ISO 960
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inEurotec
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inEurotec
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psiISO 527
Elongation at Break 3.5 %3.5 %ISO 527
Tensile Modulus 8.50 GPa1230 ksiISO 527
Izod Impact, Notched (ISO)  12.0 kJ/m²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 15.0 kJ/m²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F[10 K/min], ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 195 °C383 °FISO 75
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 250 - 270 °C482 - 518 °F
Feed Temperature 50.0 - 70.0 °C122 - 158 °FThroat
Mold Temperature 60.0 - 100 °C140 - 212 °F
Drying Temperature 120 °C248 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.080 %<= 0.080 %ISO 960
Hold Pressure 40.0 - 80.0 MPa5800 - 11600 psi
 
Descriptive Properties
Back PressureLow
Injection SpeedFast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Edinburg Plastics BTA706 PBT, Impact Modified
Chang Chun Plastic PBT3030 30% Glass Fiber Enforced PBT
Celanese Crastin® HR5330HFS NC010 PBT-IGF30
BLUESTAR 403G-MG30 PBT, 30% Glass Filled
RTP Company RTP 1000 HI Polybutylene Terephthalate (PBT) Impact Modified

PEUROS108 / 147098

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.