MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil Exceed™ 1518EC Tough Premium Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Blow Molding Grade

Material Notes: Exceed 1518EC resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518EC resin have outstanding tensile, impact strength and puncture. These superior strength properties, along with excellent drawability, allow downguaging.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ExxonMobil Method
Thickness 25.4 microns1.00 mil
Melt Flow 1.5 g/10 min1.5 g/10 minExxonMobil Method
Antiblock Level 5000 ppm5000 ppm
Slip Level 800 ppm800 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 8.96 MPa1300 psiat 2% offset; ASTM D882
Film Tensile Strength at Yield, TD 8.96 MPa1300 psiat 2% offset; ASTM D882
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 570 %570 %ASTM D882
Puncture Energy 1.59 J1.17 ft-lbExxon Mobil Method
Elmendorf Tear Strength, MD 12.6 g/micron320 g/milASTM D1922
Elmendorf Tear Strength, TD 18.5 g/micron470 g/milASTM D1922
Dart Drop 21.3 g/micron540 g/milASTM D1709
Film Tensile Strength at Break, MD 39.3 MPa5700 psiASTM D882
Film Tensile Strength at Break, TD 32.4 MPa4700 psiASTM D882
1% Secant Modulus, MD 179 MPa26000 psiASTM D882
1% Secant Modulus, TD 185 MPa26900 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 119 °C246 °FPeak Melting Temperature; ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 21 %21 %ASTM D1003
Gloss 36 %36 %45°, MD; ASTM D2457
 40 %40 %45°, TD; ASTM D2457
 
Descriptive Properties
FeaturesPPA and Thermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEXB122 / 37427

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.