MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Arla RPC™ PC Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: Arla Plast RPC™ is a range of opaque colored polycarbonate sheets. The product is virtually unbreakable with extremely high impact resistance. The product offers high temperature performance. RPC is mainly extruded in black color for thermoforming purposes. The sheet has a base regrind material which is then covered with a co-extruded top layer as in the MAKROTECH® range. Carbon black offers excellent UV absorbance which projects the material for outdoor applications. The product offers good cost savings versus performance.

Benefits: Environmental friendly with recycled core; Good impact resistance; Wide temperature range

Application: Indoor applications as flat, curved and formed parts automotive agricultural, covers and containers

Information provided by Arla Plast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ISO 2039-2
Tensile Strength, Yield 50.0 MPa7250 psiISO 527
Elongation at Break >= 50 %>= 50 %ISO 527
Elongation at Yield 6.0 %6.0 %ISO 527
Modulus of Elasticity 2.30 GPa334 ksiISO 527
Flexural Strength >= 90.0 MPa>= 13100 psiISO 178
Flexural Modulus 2.30 GPa334 ksiISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) NBNBISO 180/1U
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FDIN 53516
Vicat Softening Point 149 °C300 °FB 120; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARLA927 / 301105

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.