MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® resins are formulated for filament winding applications serving the composite pressure vessel, tank, and piping markets. These PU resins have tested positively in both hot and cold pressure vessel applications and can be applied to reinforce thermoplastic substrates (i.e. polyethylene, ABS, etc.) or applied directly to a release coated mandrel surface.

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 100 - 300 cP
@Temperature 75.0 °C
100 - 300 cP
@Temperature 167 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 89.0 MPa12900 psiPlain Cast Resin; ASTM D638
Elongation at Break 5.0 - 6.0 %5.0 - 6.0 %Plain Cast Resin; ASTM D638
Modulus of Elasticity 3.00 GPa435 ksiPlain Cast Resin; ASTM D638
Flexural Yield Strength 115 MPa16700 psiPlain Cast Resin; ASTM D790
Flexural Modulus 2.80 GPa406 ksiPlain Cast Resin; ASTM D790
Izod Impact, Notched 4.78 J/cm8.95 ft-lb/inPlain Cast Resin; ASTM D256
Charpy Impact, Notched 0.230 J/cm²1.09 ft-lb/in²Plain Cast Resin
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 136 °C277 °FPlain Cast Resin; ASTM D648
Glass Transition Temp, Tg 145 °C293 °FPlain Cast Resin; ASTM D3418
 
Processing PropertiesMetricEnglishComments
Pot Life 40.0 - 60.0 min
@Temperature 23.0 °C
40.0 - 60.0 min
@Temperature 73.4 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Isoplast® 101LGF40BLK Engineering Thermoplastic Polyurethane Resin
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
Lubrizol Isoplast® 202LGF40 Engineering Thermoplastic Polyurethane Resin
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin
Overview of materials for Thermoset Polyurethane, Liquid

PMILL000f / 159592

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.