MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company PermaStat® 301 TFE 10 Polycarbonate (PC), Glass Fiber - PTFE Lubricated - ESD Protection - Permanently Anti-static
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Glass + PTFE Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D 792
Filler Content 10 %10 %Primary Additive
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
@Thickness 3.17 mm
0.0030 - 0.0050 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 44.8 MPa6500 psiASTM D 638
Elongation at Break 7.0 - 10 %7.0 - 10 %ASTM D 638
Tensile Modulus 2.76 GPa400 ksiASTM D 638
Flexural Strength 68.9 MPa10000 psiASTM D 790
Flexural Modulus 2.41 GPa350 ksiASTM D 790
Izod Impact, Notched 1.33 J/cm
@Thickness 3.17 mm
2.50 ft-lb/in
@Thickness 0.125 in
D 256
Izod Impact, Unnotched 13.3 J/cm
@Thickness 3.17 mm
25.0 ft-lb/in
@Thickness 0.125 in
ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+9 - 9.90e+10 ohm-cm1.00e+9 - 9.90e+10 ohm-cmASTM D 257
Surface Resistance 1.00e+9 - 9.90e+10 ohm1.00e+9 - 9.90e+10 ohmESD STM11.11
Surface Resistivity per Square 1.00e+10 - 9.90e+11 ohm1.00e+10 - 9.90e+11 ohmASTM D 257
Static Decay <= 2.0 sec<= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 221 - 243 °C430 - 470 °F
Mold Temperature 65.6 - 121 °C150 - 250 °F
Drying Temperature 121 °C250 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 41.4 - 68.9 MPa6000 - 10000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polykemi AB SCANTEC PC S75R GF20 Polycarbonate, Glass Fiber Reinforced
MRC Polymers NAXELL™ PC23M-20G General Purpose Low Viscosity Polycarbonate 20% Glass Fiber Reinforced
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
LNP Lubricomp® DFL-4032 BK8-250 Polycarbonate, Glass Fiber Reinforcement, PTFE Lubricant
Kotec Carbotex KGN-20MRA Polycarbonate, Flame Retardant, 20% Glass Fiber Reinforced

PQZWA2587 / 91248

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.