MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

94.5Pb-5.5Ag Lead-Silver Solder, ASTM Class 5.5S; UNS L50180
Categories: Metal; Nonferrous Metal; Lead Alloy; Solder/Braze Alloy

Key Words: Solder Alloy Grade Ag5.5, AMS 4755, FED QQ-S-571 (Ag5.5)
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 11.3 g/cc0.408 lb/in³Calculated
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 32.0 MPa4640 psi
Elongation at Break 28 %28 %in 50 mm
 
Thermal PropertiesMetricEnglishComments
Melting Point 304 - 343 °C579 - 649 °F
Solidus 304 °C579 °F
Liquidus 343 °C649 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0050 %<= 0.0050 %
Antimony, Sb <= 0.40 %<= 0.40 %
Arsenic, As <= 0.020 %<= 0.020 %
Bismuth, Bi <= 0.25 %<= 0.25 %
Cadmium, Cd <= 0.0010 %<= 0.0010 %
Copper, Cu <= 0.30 %<= 0.30 %
Iron, Fe <= 0.0020 %<= 0.0020 %
Lead, Pb 94.5 %94.5 %nominal
Other <= 0.030 %<= 0.030 %
Silver, Ag 5.0 - 6.0 %5.0 - 6.0 %
Tin, Sn <= 0.25 %<= 0.25 %
Zinc, Zn <= 0.0050 %<= 0.0050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
94.5Pb-5Sn-0.5Ag Lead-Tin-Silver Solder
60-40 Soft Solder (60 Sn-40Pb) - ASTM B 32 Grade Sn60
5/95 Solder (95Pb-5Sn), UNS L54320
98.5Pb-1.5Ag Lead-Silver Solder, UNS L50132
10/90 (90Pb-10Sn) Solder - ASTM B32 Grade Sn10A, UNS L54520

MLSAg6 / 12248

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.