PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS 1415 has excellent mechanical properties and is easy to extrude. Applications: Extrusion of multi-layer sheet with natural HIPS, ABS or conductive or natural TPE. Processing PRE-ELEC® ABS 1415 compound can be processed in the machines using normal processing conditions as with ABS. Test Specimen: 10[mm] wide moulded rod Information from Premix OY |