MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Spartech Acrylloy 10 Acrylic Sheet
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: Description: Acrylic Sheet

Information provided by Spartech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 106106ASTM D785
Tensile Strength, Yield 37.9 MPa5500 psiASTM D638
Tensile Modulus 1.52 GPa220 ksiASTM D638
Flexural Yield Strength 71.0 MPa10300 psiASTM D790
Flexural Modulus 1.86 GPa270 ksiASTM D790
Izod Impact, Unnotched 0.587 J/cm1.10 ft-lb/inASTM D256
Falling Dart Impact 13.6 J10.0 ft-lb73°F; ASTM D3029
 
Thermal PropertiesMetricEnglishComments
CTE, linear 101 µm/m-°C
@Temperature 20.0 °C
56.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C170 °FASTM D648
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Gloss 90 %90 %Gardner; ASTM D2523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm PLEXIGLAS® Optical POQ64 PMMA
Röhm XT® Polymer 2000-5052 Acrylic-Based Multipolymer Molding Compound
Röhm PLEXIGLAS® Optical POQ62 PMMA
Röhm ACRYLITE® Grey 7D006 RP Optical PMMA (High Resolution)
Plaskolite Optix® SG Sign Grade Acrylic Sheet

PSPAR000 / 68441

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.