MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 Kendall® Hyken® 052 Farm Tractor Lubricant
Categories: Fluid; Lubricant

Material Notes: Kendall® Hyken 052 is a multifunctional fluid specially formulated for use in farm tractors and other off-highway equipment requiring one lubricant for the transmission, final drive, wet brakes and hydraulic systems. It meets the performance requirements of all major brands of farm tractors and other farm equipment that utilize a common fluid reservoir. Hyken 052 is formulated to provide excellent oxidation resistance, excellent wear protection, protection against rust and corrosion, and resistance to foaming. It has carefully balanced frictional properties to ensure proper operation of wet brakes and transmission clutches. Hyken 052 is available in two viscosity grades for use over a wide range of temperatures. The heavier viscosity grade is suitable for year-round use in most climates, whereas the “Low Viscosity” grade is recommended for use in cold climates where a John Deere J20D fluid is specified.

Applications: Hyken 052 is recommended for use where the equipment manufacturer specifies:

  • AGCO Power Fluid 821XL, Q-1826, Q-1802 (Type 55 Fluid), Q-1766B
  • Case IH MS1210, MS1209, MS1207, MS1206
  • Case New Holland (CNH) MAT3525 (134-D Fluid), MAT3506, MAT3505
  • Caterpillar TO-2 (obsolete)
  • Denison Hydraulics HF-0, HF-1, HF-2
  • Ford ESN-M2C134-D, ESN-M2C86-C, ESN-M2C86-B, ESN-M2C41-B
  • Ford-New Holland FNHA-2-C-201.00
  • John Deere JDM J20C, J20D(“Low Viscosity” grade), J14C(Type 303 Fluid)
  • Kubota UDT Fluid
  • Landini Tractor II Hydraulic Fluid
  • Massey Ferguson CMS M1145/M1143, M1141, M1135, M1129A
  • Sundstrand Hydrostatic Transmission Fluid
  • Vickers (Eaton) M-2950-S, I-286-S
  • Volvo VME WB 101 (VCE 1273.03)
  • ZF TE-ML 03E, 05F, 17E
Hyken 052 also meets API GL-4 performance requirements.

Features/Benefits:

  • Excellent oxidation resistance and thermal stability
  • Excellent wear protection for clutches, gears and hydraulic pumps
  • Prevents brake chatter and grabbing
  • Protects against rust and corrosion
  • Excellent seal compatibility
  • Good foam resistance
  • Two viscosity grades for use in most climates

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Brookfield Viscosity
  • Brookfield Viscosity
  • Viscosity Measurement, Index
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Ash, ASTM D874, Sulfated
  • ASTM Color, ASTM D1500
  • Total Base Number, ASTM D2896
  • Pour Point
  • Flash Point, COC
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.