MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
SEKISUI SPI KYDEX® 7200ST Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: Smoke and toxicity compliant aviation sheet

KYDEX® 7200ST is a high performance thermoplastic sheet designed for use in aviation interior applications where smoke and ABD0031 or BSS7239 toxicity compliance is required

KYDEX® 7200ST meets the flammability and smoke development requirements set forth in Federal Aviation Regulations (FAR) 25.853 paragraphs (a) and (d) Part V as well as the toxicity requirements for Airbus (ABD0031) and Boeing (BSS7239). Its wide processing window and ease of thermoforming makes it ideal for complex parts.

Suggested Applications:

  • Armrests
  • Tray tables
  • Kick panels
  • Trim parts

Features:

  • Meets flammability and smoke development requirements listed in FAR 25.853(a) and (d) Part V
  • Compliant to ABD0031 and BSS7239 toxicity specifications
  • Excellent formability and fabrication characteristics
  • Allows for tight tolerance control
  • Available in P3 - Velour Matte in thicknesses from 1.19 mm to 4.75 mm (0.047 in to 0.187 in)

Values based upon 0.125 in (3.18 mm) sheet unless otherwise specified.

Information provided by Sekisui Polymer Innovations

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption, ASTM D570
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Yield Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Ultimate Bearing Strength, ASTM D953
  • Bearing Yield Strength, ASTM D953, 4% deflection
  • Shear Strength, ASTM D732
  • Gardner Impact, ASTM D5420
  • Dielectric Strength, ASTM D149, oil
  • CTE, linear, Transverse to Flow, ASTM E831
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed/Annealed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.