MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Carpenter S7 Alloy Tool Steel (AISI S7)
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel; Hot Work Steel

Material Notes: Carpenter S7 is a general purpose air hardening tool steel having high impact and shock resistance. It has good resistance to softening at moderately high temperatures. This combination of properties makes it suitable for many hot-work and cold-work applications. It is available as a DeCarb-Free product. DCF bars have been cold finished in the mill, eliminating the need for bar bark removal. Both Carpenter S7 and Bearcat, a trademark of Bethlehem Steel Corp., have the same AISI tool steel designation . . . S7.

Information provided by Carpenter Technology Corporation.

Vendors:
Available Properties
  • Specific Gravity
  • Hardness, Rockwell C, Tempered at 1200°F
  • Hardness, Rockwell C, As hardened
  • Tensile Strength, Ultimate, when tempered at 400°F
  • Tensile Strength, Yield, when tempered at 400°F
  • Elongation at Break, when tempered at 400°F
  • Reduction of Area, when tempered at 400°F
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Transformation Temperature, Ac1
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Silicon, Si
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Carpenter Technology Corporation (Cartech)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.