MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 Kendall® Marine 2-Cycle Motor Oil
Categories: Fluid; Lubricant

Material Notes: Kendall® Marine 2-Cycle Motor Oil is a high quality, ashless engine oil specially designed for use in water-cooled and most air-cooled 2-stroke cycle engines. It is TC-W3® certified by the National Marine Manufacturers Association (NMMA), and also meets API TC and JASO FB performance requirements for use in air-cooled 2-stroke cycle engines. It is recommended for use in low- to mid-horsepower (up to 115 HP) engines, and may be used in either direct oil injection or premix engines. Marine 2-Cycle Motor Oil is formulated to minimize piston ring sticking and exhaust port deposits to maintain good power output in 2-stroke cycle engines. It also protects against piston and cylinder scuffing and helps reduce spark plug fouling and pre-ignition problems. It provides rust and corrosion protection in service and during storage. It is pre-diluted with a high-flash solvent for easy mixing with gasoline at low temperatures for premix applications.

Applications:

  • Outboard marine engines
  • Personal watercraft
  • Motorcycles, scooters, and all-terrain vehicles (ATVs)
  • Snowmobiles
  • Low-output chain saws
  • Lawn-care equipment (mowers, weed trimmers, leaf blowers)
Marine 2-Cycle Motor Oil is licensed under the following industry specification:
  • NMMA TC-W3® (Certification No. RL-13129R)
Marine 2-Cycle Motor Oil meets or exceeds the requirements of:
  • API TC
  • JASO FB
  • NMMA TC-WII®, TC-W® (obsolete specifications)
Features/Benefits:
  • Meets all outboard and personal watercraft manufacturers warranty requirements where a TC-W3® oil is specified
  • Ashless dispersant/detergent formulation helps minimize engine deposits and pre-ignition
  • Minimizes piston ring sticking and helps reduce exhaust port blocking
  • Protects against piston and cylinder scuffing
  • Good lubricity
  • Reduces spark plug fouling
  • Good rust and corrosion protection
  • Keeps engine parts clean
  • Mixes easily with gasoline at low temperatures
  • Dyed for easy visibility when mixed with gasoline
  • Suitable for either direct oil injection or premix engines(

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Ash, ASTM D874, Sulfated
  • Pour Point
  • Flash Point, PMCC
  • Flash Point, COC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.