MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Morgan Advanced Ceramics Kao-Tex™ Textile 1000 Cloth
Categories: Ceramic; Oxide

Material Notes: Kao-Tex Textile 1000 cloths are woven from a highly textured continuous filament yarn. A unique treatment is applied to the cloths that preserves texturization in fabrication use. The cloths are produced from inorganic materials that do not produce hazardous off gassing. The Kao-Tex Textile 1000 Cloths are especially designed and developed for temperatures up to 1000°F (538°C). Kao-Tex Textile 1000 cloths style 400 and 600 are lighter weight fabrics, thinner offering a more economical basic insulation. Kao-Tex Textile 1000 Cloths styles 800, 1000, 1200, 1350, 1400 and 2200 are a heavier weight fabric which offer a more superior insulation and durability.

Applications:

  • Welding, Fire, Oven and Drop curtains
  • Stress Relieving blankets
  • Fire and Heat barriers
  • Removable Insulation
  • Lagging
  • Fabric Expansion joints
  • Gasketing and Sealing
  • Gloves and Mittens

Information provided by Morgan Advanced Materials

Vendors:
Available Properties
  • Specific Gravity
  • Moisture Absorption, surface
  • Dielectric Constant
  • Dielectric Strength
  • Melting Point
  • Maximum Service Temperature, Air, Continuous Use
  • Al2O3
  • B2O3
  • CaO
  • K2O+Na2O
  • MgO
  • Other
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.