MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP34 Room Temperature Curing Two Component Epoxy System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, High Temperature

Material Notes: Key Features:
  • Resists up to +450°F
  • Easily machinable
  • Excellent dimensional stability
  • High bond strength
  • Superb electrical insulation properties
  • Two component system
Product Description: Master Bond EP34 is a two part, room temperature curing epoxy system for bonding, sealing and coating featuring high temperature resistance, sterling dimensional stability and peerless electrical insulation properties. It is also much easier to machine compared to most other epoxies. It has a 100 to 70 mix ratio by weight and a very convenient one to one ratio by volume. This system cures readily at room temperature or more rapidly at elevated temperatures. To optimize its properties, the recommended cure schedule is overnight at room temperature followed by a post cure at 150-200°F for 2-3 hours. Upon polymerization EP34 is serviceable from -60°F to +450°F. It resists a range of chemicals including water, oils, fuels and many acids and bases. This moderate viscosity system bonds well to a wide variety of substrates including metal, composites, glass, ceramics and many rubbers and plastics. As previously mentioned, it is a top notch electrical insulator and has an array of superior physical properties. EP34 is 100% reactive and does not contain any diluents or solvents. The color of Part A is gray, Part B is amber. It is widely used in aerospace, electronic, electrical and specialty OEM type applications.

Product Advantages:

  • Convenient mixing: one to one ratio by volume
  • Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly
  • High temperature resistance up to +450°F
  • Noteworthy electrical insulation properties
  • Excellent dimensional stability
  • Easily machinable
  • Superb adhesion to a wide variety of substrates

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Compressive Strength
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.