MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Morgan Advanced Ceramics HIP Vitox ™ Mac-A999R Bio Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: A very high purity alumina ceramic of 99.9% Al2O3 content, produced specifically for surgical implant devices.

Prime Features:

  • Clinical use since 1985
  • Highest levels of QA and traceability
  • Excellent wear resistance - far superior to polyethylene/metal joint systems
  • Very high density and non-porous alumina
  • Ultra fine grain
  • Resistant to extreme chemical environments
  • High mechanical strength
  • Highly cost effective
Typical Applications:
  • Joint replacement components
  • Femoral heads to match cup liners of same material or UHMWPE
  • Cup liners
Production Capabilities:
  • 28mm or 32mm diameter for –4 to +4 neck lengths
  • Femoral heads and cup liners for surgeons’ preferred hip systems.

Information provided by Morgan Advanced Materials

Key Words: Mac-A999R Bio
Vendors:
Available Properties
  • Bulk Density
  • Open Porosity, fully dense, % nominal, apparent
  • Grain Size
  • Hardness, Rockwell HR45N
  • Hardness, Vickers, [GPa]
  • Modulus of Elasticity
  • Flexural Strength, biaxial
  • Flexural Strength, 4-point
  • Fracture Toughness, KIC(SENB)
  • K Factor (Wear Factor), (mm3/Nm)10-7, in physiological saline, against UHMWPE, pin-on-plate test, 3.89 recommended ICRP dose
  • K Factor (Wear Factor), (mm3/Nm)10-7, in distilled water, against UHMWPE, pin-on plate test, 1.12 recommended ICRP dose
  • K Factor (Wear Factor), (mm3/Nm)10-7, in distilled water, against UHMWPE, in-on disc test, 0.87 recommended ICRP dose
  • K Factor (Wear Factor), (mm3/Nm)10-7, in calf bovine serum, against UHMWPE, pin-on-plate test, 1.81 recommended ICRP dose
  • K Factor (Wear Factor), (mm3/Nm)10-7 dry, against UHMWPE, pin-on-disc tests, 3.4 recommended ICRP dose
  • K Factor (Wear Factor), (mm3/Nm)10-9, 5M cycles , 100 stainless steel recommended ICRP dose
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Al2O3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.