MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
KKPC KOSYN SOL 5740 Solution Styrene Butadiene Rubber (S-SBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Solution Styrene Butadiene Rubber (S-SBR)

Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It is superior to SBR, which is made by emulsion polymerization, in processability, visco-elasticity and low temperature properties. Also, the products' properties can be adjusted to the purpose of consumption according to the proper proportion of styrene content, the micro structure and the molecular weight.

Applications: Shoes, Soles, Tires, Machine Parts, Energy-saving Tires, High-efficiency Tires

Additional Notes:
Bound Styrene: 15%
cis-1,4 Contents: 14%
trans-1,4 Contents: 28%
Vinyl Contents: 57%
Dynamic Test: GABO Qualimeter (11Hz)
(TAN) 0°C: 0.235
10°C: 0.162
60°C: 0.09
70°C: 0.084

This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants.

Data provided by Korea Kumho Petrochemical Co., Ltd.

Vendors:
Available Properties
  • Mooney Viscosity, Raw; ML1+4
  • Mooney Viscosity, ML1+4; Polymer 100, HAF Black (IRB#6) 50, ZnO 3, Stearic Acid 1, D 0.3, DM 0.6, Sulfur 1.75, Total: 156.65, Cure: 145°C, 35 minutes.
  • Hardness, Shore A, JIS-A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 300% Modulus
  • Glass Transition Temp, Tg, Compound
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Korea Kumho Petrochemical Co., Ltd.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.