MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Kazanorgsintez P2KP Polyethylene Pigment Masterbatches
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Masterbatch Grade

Material Notes: Production Method: P2KP polyethylene pigment masterbatches are produced on the basis of low density polyethylene with high content of masterbatches.

Application: P2KP polyethylene pigment masterbatches are used for coloring low density polyethylene in the extrusion process, cable insulation, and for coloring general-purpose products including food containers, as well as toy production by extrusion and jet molding methods. The following colors of polyethylene pigment masterbatches are available: white, yellow, orange, green, blue, brown, and black.

Information Provided by Kazanorgsintez

Key Words: LDPE
Vendors:
Available Properties
  • Melt Flow, on the basis of basic grades 10703-020, 10803-020, and 18503-020, for masterbatches of other applications (coloring general purpose products, coloring toys, coloring food containers
  • Melt Flow, on the basis of basic grades 10703-020, 10803-020, and 18503-020, for cable masterbatches
  • Melt Flow, on the basis of basic grades 11503-070 and 16803-070
  • Dielectric Constant, For cable masterbatches
  • Dielectric Strength, For cable masterbatches, at alternating voltage frequency
  • Dissipation Factor, For cable masterbatches
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.