MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Eastman NPG™ Glycol Platelets
Categories: Other Engineering Material

Material Notes: Product Description: Eastman NPG™ glycol is the industry standard glycol component in high-quality polyester resins for industrial coatings and fiberglass-reinforced plastics applications. Most polyester resin formulations contain NPG as the sole glycol component, or it is used in conjunction with a modifying glycol to achieve desired properties. NPG and Eastman™ PTA (Purified Terephthalic Acid) are the primary components for polyester powder coating resins. Eastman NPG™ delivers the overall toughness, stain and detergent resistance, and outdoor weathering performance required of coil coatings for appliances and products for exterior applications. Gel coats containing unsaturated polyesters made from NPG and Eastman™ PIA (Purified Isophthalic Acid) provide excellent weatherability and water and stain resistance. Eastman NPG™ is also used in polyester polyols for polyurethane coatings for the automotive, industrial maintenance, transportation, and aerospace markets.

Application/Uses:

  • Automotive OEM
  • Intermediate for plasticizers
  • Intermediate for synthetic lubricants
  • Polyester polyols for polyurethane coatings
  • Polyester powder coating resins
  • Polyols for rigid and flexible polyurethane foams
  • Reactive polyesters for melamine crosslinked high-solids and coil baking enamels
  • Unsaturated polyesters used in gel coats and synthetic marble
Key Attributes:
  • Excellent thermal stability for low resin color
  • Excellent weathering
  • Good chemical and stain resistance
  • Good chemical, stain, and humidity resistance
  • Good hardness/flexibility balance
  • Ideal glass transition temperature range
  • Outstanding powder flow and fluidization characteristics
  • Outstanding weathering
  • Rapid reactivity during esterification and cure

Information provided by Eastman

Vendors:
Available Properties
  • Bulk Density
  • Density
  • Molecular Weight
  • Melting Point
  • Boiling Point
  • Flash Point, Tag Closed Cup
  • Flash Point, Cleveland Open Cup
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.