MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Ineos H02C-00 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade; Polypropylene, Extrusion Grade; Polypropylene, Sheet/Thermoforming Grade

Material Notes: This is a low flow rate, high clarity homopolymer designed for extrusion, thermoforming, blow molding, and rigid packaging. Applications that require good see-through clarity combined with good heat resistance can benefit from this grade of material. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

    Applications
  • Thermoformed packaging (cups, containers, lidding)
  • Extrusion blow molded containers and bottles
  • Injection blown molded containers and bottles
  • Extruded sheet and profiles

    Benefits
  • Excellent clarity
  • Excellent processability

Information provided by Ineos Olefins & Polymers USA

Key Words: Low flow rate, high clarity
Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell R, ASTM D785, Injection Molded
  • Tensile Strength at Break, ASTM D638, 2.0 in/min, Injection Molded
  • Tensile Strength, Yield, ASTM D638, 2.0 in/min, Injection Molded
  • Elongation at Break, ASTM D638, 2.0 in/min, Injection Molded
  • Elongation at Yield, ASTM D638, 2.0 in/min, Injection Molded
  • Flexural Modulus, 1% Secant, ASTM D790A, Injection Molded
  • Izod Impact, Notched, ASTM D256, Injection Molded
  • Izod Impact, Notched (ISO), ASTM D256, Area, Injection Molded
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed, Injection Molded
  • Vicat Softening Point, ASTM D1525
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, 60°
  • Transmission, Visible, ASTM D1003, plaque, Diffuse Transmittance
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Ineos Olefins & Polymers USA

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.