MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Asahi Kasei Leona™ 54G33 Polyamide 66, GF Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Enhanced strength, stiffness, and impact resistance; with 33% GF. Excellent appearance.

Applications:Fans, railroad tie insulators, office furniture

Information provided by Asahi Kasei Corp.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792, Dry as Molded
  • Density, ISO 1183, Dry as Molded
  • Moisture Absorption at Equilibrium, ISO 62, 50% RH
  • Moisture Absorption at Equilibrium, 50% RH
  • Linear Mold Shrinkage, Flow, Asahi Kasei
  • Linear Mold Shrinkage, Transverse, Asahi Kasei
  • Hardness, Rockwell M, ISO 2039, Conditioned at 50% RH
  • Hardness, Rockwell M, ISO 2039, Dry as Molded
  • Hardness, Rockwell R, ISO 2039, Conditioned at 50% RH
  • Hardness, Rockwell R, ISO 2039, Dry as Molded
  • Tensile Strength at Break, ISO 527, Conditioned at 50% RH
  • Tensile Strength at Break, ISO 527, Dry as Molded
  • Tensile Strength, ASTM D638, Conditioned at 50% RH
  • Tensile Strength, ASTM D638, Dry as Molded
  • Elongation at Break, ISO 527, Dry as Molded
  • Elongation at Break, ISO 527, Conditioned at 50% RH
  • Tensile Modulus, ISO 527, Conditioned at 50% RH
  • Tensile Modulus, ISO 527, Dry as Molded
  • Flexural Strength, ISO 178, Conditioned at 50% RH
  • Flexural Strength, ISO 178, Dry as Molded
  • Flexural Modulus, ISO 178, Conditioned at 50% RH
  • Flexural Modulus, ISO 178, Dry as Molded
  • Izod Impact, Notched, ASTM D256, Dry as Molded
  • Izod Impact, Notched, ASTM D256, Conditioned at 50% RH
  • Charpy Impact Unnotched, ISO 179, Conditioned at 50% RH
  • Charpy Impact Unnotched, ISO 179, Dry as Molded
  • Charpy Impact, Notched, ISO 179, Dry as Molded
  • Charpy Impact, Notched, ISO 179, Conditioned at 50% RH
  • Volume Resistivity, IEC 60093, Dry as Molded
  • Surface Resistance, IEC 60093, Dry as Molded
  • Dielectric Strength, IEC 60243, Dry as Molded
  • Comparative Tracking Index, IEC 60112, Dry as Molded
  • CTE, linear, ASTMD 696, Dry as Molded
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75, Dry as Molded
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75, Dry as Molded
  • Flammability, UL94, Dry as Molded
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.