MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
KLJ Group KLJ-EPR Silane Cross-Linkable Elastomeric Compound
Categories: Polymer; Thermoplastic

Material Notes: Description: KLJ-EPR is a silane cross-linkable Elastomeric Compound, curable when exposed to moist conditions. The compound is processed in the same way as a non-curable elastomer having good extrusion properties at high output rates. The graft component KLJ-EPR is to be mixed with a Cross-Linking catalyst master batch KLJ-XL-MB-01M in the ratio 95%. It is highly flexible and enables the production of soft rubber cables without the use of Continuous Vulcanization equipment. This material is suitable to be used for cable up to 11 KV.

Specification: KLJ EPR meets the following specifications.

Information provided by KLJ Group

Vendors:
Available Properties
  • Tensile Strength, IS 10810 Part 7
  • Tensile Strength, IS 10810 Part 11
  • Elongation at Break, IS 10810 Part 7
  • Elongation at Break, IS 10810 Part 11, Cold Elongation Test
  • Elongation at Break, IS 10810 Part 11
  • Volume Resistivity, IS 3396
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60250
  • Dissipation Factor, IEC 60250
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.