Global EPP POM C Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Polyacetals are highly crystalline thermoplastics, characterised by their high mechanical strength, rigidity and impact resistance. Acetal absorbs very little moisture, enabling the product to maintain constant physical properties in a variety of changing environments. POM exhibits excellent dimensional stability and is ideally suited to close tolerance mechanical parts.

Key characteristics:

  • High mechanical strength and rigidity
  • High impact strength and creep resistance
  • Excellent dimensional stability and machinability
  • Low moisture absorption
  • Good electrical insulating and dielectric properties
  • No centreline porosity in copolymer grades
  • Suitable for food contact

The copolymer grade is the ideal combination of strength, stiffness and wear resistance. It absorbs very little moisture, is easily machinable and is genuinely porosity-free, making it the preferred grade for food contact and medical applications. The product exhibits an elevated resistance to hydrolysis, strong alkalis and thermal-oxidative degradation when compared to acetal homopolymer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³Test Method A; ISO 1183:1987
Water Absorption 0.20 %
@Temperature 23.0 °C,
Time 86400 sec
0.20 %
@Temperature 73.4 °F,
Time 24.0 hour
Immersion; ISO 62:1999 (modified)
Moisture Absorption at Equilibrium 0.10 %0.10 %50% RH; ISO 62:1999
Water Absorption at Saturation 0.90 %0.90 %ISO 62:1999
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383ISO 868:2003
Tensile Strength at Break 70.0 MPa10200 psiSample Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 15 %>= 15 %Sample Type 1B, 50 mm/min; ISO 527-1/2:1993
Modulus of Elasticity 3.10 GPa450 ksiSample Type 1B, 50 mm/min; ISO 527-1/2:1993
Flexural Strength 80.0 MPa11600 psi1.5 mm/min; ISO 178:2001
Flexural Modulus 2.60 GPa377 ksi1.5 mm/min; ISO 178:2001
Compressive Strength 110 MPa16000 psiSample Type B, 5 mm/min; ISO 604:2002
Compressive Modulus 2.60 GPa377 ksiSample Type A, 1 mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 7.20 kJ/m²3.43 ft-lb/in²Sample Type A; ISO 180:2000
Coefficient of Friction, Dynamic 0.25
@Pressure 1.75 MPa
0.25
@Pressure 254 psi
31.4 m/min
Limiting Pressure Velocity 0.100 MPa-m/sec2860 psi-ft/min
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093:1980-01
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093:1980-01
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250:1969-01
Dielectric Strength 16.5 kV/mm419 kV/inIEC 60243-1:1998-01
Dissipation Factor 0.0050
@Frequency 100 Hz
0.0050
@Frequency 100 Hz
IEC 60250:1969-01
Comparative Tracking Index 600 V600 VIEC 60112:2003-01
 
Thermal PropertiesMetricEnglishComments
CTE, linear 92.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
51.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-2:1999
Thermal Conductivity 0.310 W/m-K2.15 BTU-in/hr-ft²-°FISO 8301:1991
Melting Point 170 °C338 °F
Maximum Service Temperature, Air 90.0 °C194 °FContinuous
 140 °C284 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FISO 75
Glass Transition Temp, Tg -60.0 °C-76.0 °FISO 11359-2:1999
Flammability, UL94 HBHBIEC 60695-11-10:2003-08
 
Descriptive Properties
ColorWhite, Black, and others

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.