2195 Aluminum Composition Spec
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: This data sheet has only a limited amount of property data. Most MatWeb aluminum entries, especially entries with a specific temper in the name, have much more property data. Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A92195; Aluminium 2195; AA2195; Al2195
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.71 g/cc0.0979 lb/in³AA; Typical
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 91.9 - 94.9 %91.9 - 94.9 %As remainder
Copper, Cu 3.7 - 4.3 %3.7 - 4.3 %
Iron, Fe <= 0.15 %<= 0.15 %
Lithium, Li 0.80 - 1.2 %0.80 - 1.2 %
Magnesium, Mg 0.25 - 0.80 %0.25 - 0.80 %
Manganese, Mn <= 0.25 %<= 0.25 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.12 %<= 0.12 %
Silver, Ag 0.25 - 0.60 %0.25 - 0.60 %
Titanium, Ti <= 0.10 %<= 0.10 %
Zinc, Zn <= 0.25 %<= 0.25 %
Zirconium, Zr 0.08 - 0.16 %0.08 - 0.16 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.