Copper (II) Cyanide, Cu(CN)2
Categories: Ceramic

Material Notes: CAS Number: 14763-77-0

Physical Form: Green-Powder

Key Words: Cu(CN)2, Copper Cyanide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 115.581 g/mol115.581 g/mol
 
Descriptive Properties
SolubilityInsoluble H2O; Soluble Acid and Alkaline

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.