MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aptek 6108-PMF Epoxy Encapsulant and/or Potting Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: High temperature, rigid, electrical/electronic coating or encapsulant. Provides excellent environmental protection for continuous exposure to 220°C. Also can be used as a high temperature wire varnish/impregnant for motor stators. Available as a long pot-life, 2-component system.

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D1475
Viscosity 2400 cPSpindle #2; speed 10 rpm; ASTM D1824
Outgassing - Total Mass Loss 0.10 %Cured property; at 10E-6 torr; ASTM E595
Collected Volatile Condensable Material 0.010 %Cured property; at 10E-6 torr; ASTM E595
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88Cured property; ASTM D2240
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmCured property; ASTM D257
Dielectric Constant 3.3
@Frequency 1000 Hz
Cured property; ASTM D150
Dissipation Factor 0.0090
@Frequency 1000 Hz
Cured property; ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 72.0 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 1; Perkin Elmer TMS-2
 200 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 2; Perkin Elmer TMS-2
Maximum Service Temperature, Air 220 °C
Glass Transition Temp, Tg 165 °CCured property; Perkin Elmer TMS-2
Flash Point >= 200 °CASTM D92
 
Descriptive Properties
ColorClear Amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP125 High Temperature Resistant, Toughened Epoxy System
Henkel Loctite® 3860 Thermally Conductive Potting
Epoxy Technology EPO-TEK® 920-FL Thermally Conductive Epoxy
Trelleborg Emerson & Cuming Stycast® 2762/17M-1 Two-Component Epoxy High Service Temp Encapsulant
Trelleborg Emerson & Cuming Stycast® 5954 Two-Component Silicone High Service Temp Encapsulant

PAPTEK39 / 24201

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.