MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polynt SMC LS 3200 R20 C20 SMC, High Mechanical Properties
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: SMC LS 3200 R20 C20 is a sheet molding compound based on an unsaturated polyester resin reinforced with glass fibers. This SMC has been developed for structural parts. SMC LS 3200 R20 C20 meets mechanical and thermal properties with reduction weight of the final parts. SMC LS 3200 R20 C20 is formulated according to RoHS, REAC regulation (SVHC) and WEEE European legislation.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/ccISO 1183
Filler Content 20 %continuous glass
 20 %random glass
Water Absorption <= 0.40 %ISO 62 Met. 1
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.00 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 100 MPaLongitudinal; ISO 14125A
 400 MPaTrasversal; ISO 14125A
Flexural Modulus 6000 MPaLongitudinal; ISO 14125A
 19000 MPaTrasversal; ISO 14125A
Charpy Impact Unnotched 180 kJ/m²Trasversal; ISO 179
 600 kJ/m²Longitudinal; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 240 °CISO 75
 
Processing PropertiesOriginal ValueComments
Mold Temperature 140 - 160 °C
Hold Pressure 1015 - 1595 psiMolding pressure
 
Descriptive Properties
Molding time40 s/mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9145 / 231740

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.