Product description: SILRES® IC 368 is a solventless, reactive, methoxyfunctional methyl-phenyl polysiloxane with a narrow molecular weight distribution. Application: SILRES® IC 368 is highly suitable for introducing a compatible silicone component into other binder systems to increase the weathering or heat resistance. Information provided by Wacker Chemie AG. |