Hostacom ERC 1218N Natural is a 8% mineral filled, polypropylene copolymer for injection molding. It combines low density with excellent stiffness, scratch resistance, flowability, good impact and dimensional stability. It is typically used for molding of automotive interior trim parts. Applications: Automotive Parts, Interior Automotive ApplicationsInformation provided by LyondellBasell. |