MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polynt SMC LS 3620 R35 AE Sheet Molding Compound High Fire Retardancy
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: SMC LS 3620 R35 AE is a sheet molding compound based on an unsaturated polyester resin, fire retardant grade, reinforced with glass fibers. This SMC has been developed for electrical application. SMC LS 3620 R35 AE joint excellent mechanical properties and excellent fire protection grade. SMC LS 3620 R35 AE is formulated according to RoHS, REAC regulation (SVHC) and WEEE European legislation.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/ccISO 1183
Filler Content 35 %ISO 11667
Water Absorption <= 0.20 %ISO 62 Met. 1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80ISO 2039-2
Flexural Strength 180 MPaISO 14125A
Flexural Modulus 9500 MPaISO 14125A
Charpy Impact Unnotched 90.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+14 ohmIEC 93
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °CISO 75
Flammability, UL94 V-0
@Thickness 1.50 mm
Glow Wire Flammability Index 960 °CIEC 695-2-1
 
Processing PropertiesOriginal ValueComments
Mold Temperature 140 - 160 °C
Hold Pressure 1015 - 1740 psiMolding pressure
 
Descriptive Properties
Molding time40 s/mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9142 / 231737

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.