MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
PolyMirae Clyrell EC310K Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Clyrell EC310K is a medium flow heterophasic copolymer selected by customers for use in film applications. Films produced with Clyrell EC310K shows very good gel level and good heat seal properties. Clyrell EC310K films are also characterized by an excellent balance of toughness, low temperature impact, mechanical properties, easy processing and low stress whitening. Clyrell EC310K is typically used by customers for lamination, adhesive tapes, labeling films, thermoformed containers, stationery and protective films and food packaging. Clyrell EC310K contains no slip or antiblocking agents. Clyrell EC310K is suitable for food contact.

Product Features: Very low gel content/Absence of film stress whitening/ Good film stiffness with low temperature impact/ Low blooming even after ageing/ Good seal strength/ Good optical properties/High heat resistance

Typical Applications: Extrusion of films for lamination/Adhesive tapes/ Labeling films/Thermoformed containers /Stationery /Protective films /Food packaging

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASMT D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 280 kg(f)/cm²ASTM D638
Elongation at Yield 10 %ASTM D638
Flexural Modulus 11400 kg(f)/cm²ASTM D790
Izod Impact, Notched 2.00 kg-cm/cm
@Temperature -20.0 °C
ASTM D256
 11.0 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
IRPC Polimaxx Polene 2341TC Polypropylene Block Copolymer
IRPC Polimaxx Polene 2340TC Polypropylene Block Copolymer
IRPC Polimaxx Polene 2340S Polypropylene Block Copolymer
Inno-Comp INNOPOL® CS 4-8000 Polypropylene Random Copolymer
Inno-Comp INNOPOL® CS 2-8000 Polypropylene Block-Copolymer

PMIRAF08 / 183229

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.