System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Epoxyset Epoxiohm EO-98HT Electrically Conductive Epoxy Adhesive
Categories:
Polymer
;
Adhesive
;
Thermoset
;
Epoxy
;
Epoxy, Electrically Conductive
Material Notes:
EO-98HT is a one component, electrically and thermally conductive, snap cure, die attach epoxy. It was designed for IC plastic packaging of semiconductors, hybrid micro-electronics, and photonic device assembly.
Information provided by Epoxyset Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
3.50
g/cc
Viscosity
35000
-
55000
cP
Mechanical Properties
Original Value
Comments
Hardness, Shore D
84
ASTM D2240
Shear Strength
23.0
MPa
Adhesive Bond Strength
>=
1200
psi
Lap Shear Strength
Electrical Properties
Original Value
Comments
Electrical Resistivity
<=
0.000400
ohm-cm
Thermal Properties
Original Value
Comments
CTE, linear
42.0
µm/m-°C
Thermal Conductivity
1.80
W/m-K
Maximum Service Temperature, Air
>=
200
°C
Minimum Service Temperature, Air
-55.0
°C
Glass Transition Temp, Tg
>=
110
°C
Processing Properties
Original Value
Comments
Cure Time
0.167
hour
@Temperature 175 °C
2.00
hour
@Temperature 125 °C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® OG116-31 UV Cure Optical Epoxy
Epoxy Technology EPO-TEK® OG603 UV Cure Optical Epoxy
Master Bond EP42HT-2 Epoxy Adhesive Resists Sterilization
Vitro Minerals WhiteLite™ 32 Lightweight Mineral Powder
Overview of materials for Epoxy/Carbon Fiber Composite
PEPOXY819 / 150844
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.