MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® 3565 High performance epoxy, high Tg and low CTE High Tg Underfill
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.

Loctite® Underfills and Encapsulants improve assembly operations by providing superior reliability and faster throughput. Improved reliability is achieved through products that have a high Tg, low CTE, high throughput and excellent adhesion. Faster throughput and higher yields are achieved through faster flow characteristics and increased cure speeds.

Loctite® 3565 High performance epoxy, high Tg and low CTE High Tg Underfill
A high performance underfill for flip chip devices. Specifically formatted for high reliability, hybrid and MCM applications. Designed for gaps down to 1 mil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.74 g/cc
Viscosity 45000 cPHaake cone and plate rheometer @ 5/sec (35mm/2° cone)
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 500000 psi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µm/m-°C
@Temperature 20.0 °C
Glass Transition Temp, Tg 155 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hour
@Temperature 150 °C
Full Cure
Shelf Life 3.00 Month
@Temperature -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® 3566 Rapid Flow Low Profile Underfill
Henkel Loctite® 3564 Fast flow epoxy, moderate CTE and Tg Fast Flow Underfill
Henkel Loctite® 3563 Epoxy Snap Cure Underfill
Henkel Loctite® 3534 Glob Top Encapsulant
Master Bond EP30LTE Low Thermal Expansion, Dimensionally Stable Epoxy

PLOCT186 / 51922

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.