MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV 3160 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 3100 series are engineered materials designed primarily general purpose, automotive and industrial applications requiring a good balance of thermal, mechanical, and physical properties. Sarlink 3160, available in NAT and BLK, is a medium hardness, low density, multi-purpose thermoplastic vulcanizate that can be processed by injection molding, blow molding or extrusion for applications such as grips, seals, gaskets, profiles, hose & tubes, bellows, and other articles.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Bondability; Chemical Resistant; General Purpose; Good Adhesion; Good Flexibility; Good Moldability; Good Processability; Good Surface Finish; High Elasticity; Medium Heat Resistance; Low Density; Medium Hardness; Resilient; Weather Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Interior Parts; Automotive Under the Hood; Diaphragms; Gaskets; General Purpose; Industrial Applications; O-rings; Pipe Seals; Plugs; Profiles; Rubber Replacement; Seals; Weatherstripping

Agency Ratings: UL 94; UL QMFZ2; UL QMFZ8

RoHS Compliance: RoHS Compliant

Automotive Specifications: BMW Unspecified Color: Black; CHRYSLER MS-AR-80 Type B Color: Black; CHRYSLER MS-AR-80 Type B Color: Natural; Daimler DBL 5562.30 Color: Black; FORD WSD-M2D379-A1 Color: Black; GM QK 003521 Color: Black; GM QK 003521 Color: Natural; PSA Peugeot-Citroen B62 0300 version G Color: Black; SAE J3000 Color: Black; SAE J3000 Color: Natural

UL File Number: QMFZ2.E54709

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D792
Viscosity 310 cP
@Shear Rate 206 1/s,
Temperature 200 °C
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 62
@Time 5.00 sec
Extruded; ISO 868
 65
@Time 5.00 sec
Injection Molded; ISO 868
Tensile Strength at Break 783 psiFlow; ISO 37
 914 psiAcross Flow; ISO 37
 877 psi
@Treatment Temp. 135 °C,
Time 360000 sec
Across Flow, Change in Air; ISO 188
 905 psi
@Treatment Temp. 150 °C,
Time 605000 sec
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain 363 psi
@Strain 100 %
Across Flow; ISO 37
 551 psi
@Strain 100 %
Flow; ISO 37
 374 psi
@Strain 100 %,
Treatment Temp. 135 °C
Across Flow, Change in Air, 1000 hr; ISO 188
 388 psi
@Strain 100 %,
Treatment Temp. 150 °C
Across Flow, Change in Air, 168 hr; ISO 188
Elongation at Break 270 %Flow; ISO 37
 640 %Across Flow; ISO 37
 570 %
@Treatment Temp. 150 °C,
Time 605000 sec
Across Flow, Change in Air; ISO 188
 608 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
Across Flow, Change in Air; ISO 188
Tear Strength 180 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set 23 %
@Temperature 22.8 °C,
Time 79200 sec
ISO 815
 34 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 55 %
@Temperature 90.0 °C,
Time 252000 sec
ISO 815
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.52 mm
All Colors
 
Processing PropertiesOriginal ValueComments
Processing Temperature 365 - 428 °FInjection, Melt
Rear Barrel Temperature 356 - 419 °FInjection
Middle Barrel Temperature 356 - 419 °FInjection
Front Barrel Temperature 356 - 419 °FInjection
Nozzle Temperature 369 - 428 °FInjection
Zone 1 356 - 392 °FExtrusion
Zone 2 356 - 401 °FExtrusion
Zone 3 369 - 410 °FExtrusion
Zone 4 369 - 410 °FExtrusion
Die Temperature 383 - 419 °FExtrusion
Melt Temperature 383 - 419 °FExtrusion
Mold Temperature 50.0 - 131 °FInjection
Drying Temperature 180 °F
Dry Time 3.00 hour
Back Pressure 14.5 - 145 psiInjection
Screw Speed 100 - 200 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1142 / 237633

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.