MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® H70E Thermally Conductive, Electrically Insulating Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Product Description: EPO-TEK® H70E is a two component, thermally conductive, electrically insulating epoxy designed for chip bonding in microelectronic and optoelectronics applications.

Advantages & Application Notes:

  • Heat-sinking adhesive. It is particularly recommended for thermal management applications where good heat dissipation is necessary.
  • The excellent handling characteristics and the long pot life at room temperature for this unique, two component system is obtained without the use of solvents.
  • Easy to use. It can be screen printed, machine dispensed, stamped, or hand applied.
  • Die-attach adhesive designed to be used in the 300°C range to resist TC wire bonding operations. Meets JEDEC Level III and II packaging criteria.
  • Excellent adhesion to ferrous and non-ferrous metals, lead-frame die paddle, glass, ceramic, kovar, and PCB.
  • Can be cured very rapidly; excellent material to use for making fast circuit repairs; can be snap-cured for in-line semiconductor die-bonding.
  • Passes NASA low outgassing standard ASTM E595 with proper cure

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccPart A
 2.50 g/ccPart B
Particle Size <= 50 µm
Viscosity 4000 - 7000 cP
@Temperature 23.0 °C
50 rpm
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Cl (Chloride) 186 ppm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83
Tensile Modulus 787350 psiStorage
Shear Strength >= 2000 psiLap
 >= 3400 psiDie
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cm
Dielectric Constant 4.22
@Frequency 1000 Hz
Dissipation Factor 0.0040
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 µm/m-°CBelow Tg
 64.0 µm/m-°CAbove Tg
Thermal Conductivity 0.900 W/m-K
Maximum Service Temperature, Air 200 °CContinuous
 300 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 80.0 °CDynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Decomposition Temperature 451 °CDegradation Temperature
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 min
@Temperature 175 °C
Minimum Bond Line
 5.00 min
@Temperature 150 °C
Minimum Bond Line
 15.0 min
@Temperature 120 °C
Minimum Bond Line
 90.0 min
@Temperature 80.0 °C
Minimum Bond Line
Pot Life 3360 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Descriptive Properties
ColorBeigePart B
 GrayPart A
ConsistencySlightly pourable paste
Mix Ratio by Weight1:1
Number of ComponentsTwo
Thixotropic Index1.17
Weight Loss0.24%200°C
 0.75%250°C
 1.6%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H61LV Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H61ND Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H63 Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® B9021-13 Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® 930-1 Thermally Conductive, Electrically Insulating Epoxy

PPOXYT071 / 141110

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.