MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DSM Fibre Intermediates Nyrim® 1500 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) technology. Nyrim® is a registered trademark.

Information provided by the manufacturer, Brueggemann Chemical.

Key Words: RIM materials
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 77ISO 868
Tensile Strength, Ultimate 54.0 MPaISO 527
Elongation at Break 90 %ISO 527
Modulus of Elasticity 2.106 GPaISO 527
Flexural Modulus 2.279 GPaISO 178
Poissons Ratio 0.32Calculated
Shear Modulus 0.800 GPatorsional
Izod Impact, Notched (ISO) 1.90 J/cm²ISO 180, Ductile break
 0.900 J/cm²
@Temperature -40.0 °C
Brittle break; ISO 180
Charpy Impact, Notched 2.00 J/cm²DIN 53453, Brittle break
 1.40 J/cm²
@Temperature -40.0 °C
Brittle break; DIN 53453
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 500 VDIN IEC 112 / VDE 030 t1
 
Thermal PropertiesOriginal ValueComments
Melting Point 214 °CDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Brueggemann Chemical Nyrim® 1000 (Dry)
Elastomer Engineering Elastamide 100 Elastomer Modified RIM Nylon 6
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 20 pcf, MDI-based 2-Component Liquid System
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 30 pcf, MDI-based 2-Component Liquid System
Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System

PDSMN010 / 31479

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.