MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LG Chemical LUTENE-H ME8000 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Description: LUTENE-H ME8000 is mainly intended for injection molding of containers. It has good mechanical properties and high productivity.

Applications: Silicone cartridge, containers, complicated parts, toys

CAS No. 9002-88-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.957 g/ccASTM D1505
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength, Yield 290 kg(f)/cm²ASTM D638
Elongation at Break >= 1000 %ASTM D638
Flexural Modulus 10500 kg(f)/cm²ASTM D790
Izod Impact, Notched 6.00 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Crystallization Temperature 134 °CMelting; DSC
Vicat Softening Point 125 °CASTM D1525
Shrinkage 1.5 - 5.0 %Depending on the processing conditions
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °CResin, Injection Molding
Mold Temperature 10.0 - 60.0 °CInjection Molding
Back Pressure 0.500 - 15.0 MPaInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUTENE-H ME6000 HDPE
LG Chemical LUTENE-H ME2500 HDPE
LG Chemical LUPOY NS5000 PC/ABS, High Impact
LG Chemical LUPOY NS5000C PC/ABS, High Impact
LG Chemical LUTENE-H ME1000 High Density Polyethylene

PLAY198 / 148208

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.