MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Schmolz + Bickenbach UGICHROM 4507 Duplex Chrome Plated Bar
Categories: Metal; Ferrous Metal; Duplex

Material Notes: Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced grades

Advantages: Zero defects guarantee; Low friction coefficient; High resistance to wear; Improved corrosion resistance; Micro-fissured chromium (1000 micro-fissures / cm²) guarantees a definitive level of resistance to extreme conditions in severe environments; Improved machinability (up to +20% of productivity); Superior mechanical properties; and High level of geometrical and dimensional precision

Information provided by Schmolz + Bickenbach

Key Words: EN 10088-3 1.4507; X2CrNiMoCu25-6-3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 900
@Thickness 0.100 mm
Tensile Strength at Break 760 - 890 MPa
Tensile Strength, Yield >= 550 MPa
@Strain 0.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
316 Stainless Steel, annealed bar
MetalTek MTEK 2507 Cast UNS J93404 Duplex Stainless Steel
MetalTek MTEK 29M Cast UNS J93370 Duplex Stainless Steel
Outokumpu 4313 Martensitic Stainless Steel

NSCHMO062 / 125935

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.