MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

(Viewing data as-entered. Click here to return)
Saint-Gobain Meldin® 4320 Molded Wear Grade Polyamide-Imide
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes: Wear grade mainly used for washers when wear reduction and extended lifetime of the component are key.

All 4000 series compounds have common properties that make them suitable replacements for metal components: they are stiff and retain high mechanical strength at elevated temperatures; they are very durable even in harsh applications in regards to wear; and they are chemically compatible with all automotive fluids (fuels and oils).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccASTM D792
Water Absorption 0.17 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 50.0 MPa
@Temperature 204 °C
ASTM D638
 70.0 MPa
@Temperature 150 °C
ASTM D638
 85.0 MPa
@Temperature 100 °C
ASTM D638
 108 MPa
@Temperature 23.0 °C
ASTM D638
Elongation at Break 2.4 %ASTM D638
Tensile Modulus 7.20 GPaASTM D638
Flexural Strength 67.0 MPa
@Temperature 235 °C
ASTM D790
 173 MPa
@Temperature 23.0 °C
ASTM D790
Flexural Modulus 8.30 GPaASTM D790
Compressive Strength 71.0 MPa
@Temperature 235 °C
ASTM D695
 129 MPa
@Temperature 23.0 °C
ASTM D695
Compressive Modulus 5.60 GPaASTM D695
 
Thermal PropertiesOriginal ValueComments
Melting Point 371 °CASTM D3418
Glass Transition Temp, Tg 280 °CASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTGQZ108y / 305348

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.