MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Devcon® Ultra Quartz™ Floor Patching System
Categories: Other Engineering Material

Material Notes: A heavy-duty, premium floor patching system (includes primer). Uses: Used to repair concrete in chemical environments where heavy concentrations of acids, alkalis, and hydrocarbons are destroying the floor. Ideal for rebuilding floors around acid dip tanks, pump pads, and secondary containment areas. Features: Trowelable to a non-porous finish, 9000 psi compression strength, Superior adhesion to cured concrete, Non-sag formulation, Outstanding resistance to acids, alkalis, water, oils, solvents, chemicals.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 95
Compressive Strength 9000 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °FTemperature Resistance - Wet
 250 °FTemperature Resistance - Dry
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 90.0 °FApplication Temperature
Cure Time 16.0 hour
@Temperature 24.0 °C
Functional cure
 168 hour
@Temperature 24.0 °C
As Tested
Pot Life 60.0 min
@Temperature 23.9 °C
 
Descriptive Properties
Aggregate/Liquid Ratio10:1By weight. Uncured
Chemical/Solvent ResistanceAmmonia: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Chlorinated Solvent: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Kerosene: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Methanol: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Toluene: excellent30 day immersion at 75°F. Sample cured 7 days at RT
ColorLight SandCured
Coverage13 ft²Cured. @ 1/4"
Mix Ratio by weight2:1Resin/Hardener
Recoat Time6 to 8 hrs
ViscosityPutty-paste. Mixed.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWD9214 / 239723

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.