EB-347 is a highly filled, low coefficient expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensional stability and excellent chemical resistance.Information provided by Epoxyset Inc. |