MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ecomass® 5100TU96 Tungsten Filled SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE; Styrene-Butadiene

Material Notes: Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.
  • High Specific Gravity
  • Tungsten Powder Filled SEBS Base Resin
  • Very Flexible

Information provided by Technical Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 11.0 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 23ASTM D2240
Tensile Strength, Ultimate 196 psiASTM D638
Elongation at Break 177 %ASTM D638
Flexural Strength 386 psiASTM D790
Flexural Modulus 13300 psiASTM D790
Izod Impact, Notched 2.00 ft-lb/inASTM D256
 
Processing PropertiesOriginal ValueComments
Melt Temperature 300 - 400 °F
Mold Temperature 70.0 - 100 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 199 X 108940 B Polypropylene (PP), High Gravity Compound
RTP Company RTP 199 X 108940 C Polypropylene (PP), High Gravity Compound
Ecomass® 705ZD70 Tungsten Filled ABS
Ecomass® 4450CI86 Carbonyl Iron Filled Polypropylene
Ecomass® 3608TU96 Tungsten Filled Polyethylene

PECOM15 / 35425

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.